Sillitin / Sillikolloid
The following tables show the most significant product characteristics and the pertinent test methods for Sillitin and Sillikolloid. The figures given should be understood as approximate. Specification ranges as currently guaranteed are listed under Material Specifications . They are part of our Sales Conditions.
| Characteristics | Unit | Method | Sillitin V 85 | Sillitin V 88 | Sillitin N 82 | Sillitin N 85 | Sillitin N 87 | Sillitin Z 86 | Sillitin Z 89 | Sillikolloid P 87 |
|---|---|---|---|---|---|---|---|---|---|---|
| Brightness Y |
DIN 53 163/ | 82 | 86 | 77 | 82 | 83 | 82 | 86 | 82 | |
| Brightness Z |
DIN 53 163/ | 76 | 88 | 65 | 75 | 76 | 75 | 86 | 76 | |
| Residue > 40 µm | mg/kg |
DIN ISO 787 | 25 | 25 | 25 | 25 | 20 | 20 | 20 | 20 |
| Residue > 200 µm | mg/kg |
DIN ISO 787 | 5 | 5 | 5 | 5 | 5 | 3 | 3 | 3 |
| Volatile Matter at 105 °C | % |
DIN ISO 787 | 0.5 | 0.5 | 0.5 | 0.5 | 0.5 | 0.5 | 0.5 | 0.5 |
| Density | g/cm3 |
DIN ISO 787 | 2.6 | 2.6 | 2.6 | 2.6 | 2.6 | 2.6 | 2.6 | 2.6 |
| BET Surface Area | m2/g | DIN ISO 9277 | 8 | 8 | 11 | 10 | 10 | 11 | 10 | 12 |
| Oil Absorption | g/100 g |
DIN ISO 787 | 45 | 45 | 45 | 45 | 45 | 55 | 55 | 55 |
| Volume Resistivity | Ωcm | DIN 53 779 | 1012 | 1012 | 1012 | 1012 | 1012 | 1012 | 1012 | 1012 |