Cable and electrical industry
Cable sheaths, cable insulation
Advantages
- very good extrusion properties
- medium to high tensile strength
- good compressive properties at high temperature
- good hot set properties
- high electrical resistivity, also after immersion in water
- avoidance of deposits on dies caused by filler
- good resistance against oil, water, acid
- very low dielectric loss, also after immersion in water, even without additional silane in the compound
Recommended Products
Guide Formulations
| 70 Shore A; EPDM; peroxide cure (M 432.0/3) | |
| 70 Shore A; EPDM; peroxide cure (M 432.0/4) | |
| 70 Shore A; EPDM; peroxide cure (M 432.0/8) | |
| 70 Shore A; EPDM; peroxide cure (M 432.0/9) | |
| Medium and high voltage cable insulation; 85 Shore A; EPDM; peroxide cure (M 613.1/6) | |
| Medium and high voltage cable insulation; 85 Shore A; EPDM; peroxide cure (M 613.1/9) | |
| Medium and high voltage cable insulation; 85 Shore A; EPDM; peroxide cure (M 613.1/15) | |
| Light-colored; 50 Shore A; EPDM; sulfur cure (RRS 29) | |
| High tensile strength; 60 Shore A; peroxide cure (K 1322) | |
| 60 Shore A; EPDM; peroxide cure (3386 K460) | |
| DIN VDE 0207 3GM2; 75 Shore A; EPDM; peroxide cure (E.1.0.003) | |
| DIN VDE 0207 EM1; 75 Shore A; EPDM; peroxide cure (E.1.0.004) | |
| DIN VDE 0207 EM1; 55 Shore A; EPDM; sulfur cure (E.1.0.005) | |
| DIN VDE 0207 EM1; 70 Shore A; EPDM; sulfur cure (E.1.0.006) | |
| Semko; 65 Shore A; EPDM; peroxide cure (E.1.0.001) | |