Machine and equipment construction
Roller coverings and printing blankets
Advantages
- very low residue > 40 µm
- good mixing and dispersion properties
- good rubber-metal adhesive strength
- excellent grinding properties
- high surface quality
- good for laser engraving
- low dynamic heat build-up
- low compression set
- good resistance against solvents, oil, water, acid
- avoidance of mold fouling caused by filler
Recommended Products
Guide Formulations
| Rice husking roller; 50 Shore D (97 Shore A); SBR/BR; sulfur cure (M 511.2/14) | |
| Paper press with high heat conductivity; 90 Shore A; NR; sulfur cure (RRS 27) | |
| Replacement for stone rollers with high heat conductivity; 40 Shore D; SBR/NR; sulfur cure (RRS 28) | |
| Resistant to animal fat, colophonic acid and offset print colors; 30 Shore A; PNR; sulfur cure (RRS 44) | |
| Resistant to animal fat, colophonic acid and offset print colors; 40 Shore A; PNR; sulfur cure (RRS 45) | |
| 20 Shore A; PNR; sulfur cure (RRS 17) | |
| 60 Shore A; EPDM; sulfur cure (RRS 22) | |
| 60 Shore A; EPDM; sulfur cure (RRS 23) | |
| 80 Shore A; EPDM; sulfur cure (RRS 24) | |
| 80 Shore A; EPDM; sulfur cure (RRS 25) | |
| 25/30 Shore A; EPDM; sulfur cure (3118 B15) | |
| 25/30 Shore A; EPDM; sulfur cure (3118 B16) | |
| Antistatic; 55 Shore A; NR/BR; sulfur cure (2828) | |
| 45 Shore A; EPDM; sulfur cure (RRS 21) | |
| Oil resistant; 80 Shore A; NBR; sulfur cure (RRS 26) | |
| 80 Shore A; NR; sulfur cure (AT11/19) | |